The epoxy resin has a limiting oxygen index (LOI) measured according to standard ASTM 2863, which is at least 28%, if the resin comprises at least a silsesquioxane compound (POSS), or at least 36%, if the resin is obtainable by curing an epoxy precursor formulation with an hardening agent which is an aromatic organo-phosphorous compound, preferably an organophosphine oxide of general formula R 3 PO, wherein at least two R moieties are amino-phenyl and one R moiety is alkyl, phenyl or amino-phenyl, wherein each phenyl ring may have independently one or more electrophile substituents.

Multifunctional epoxy resin with enhanced flame resistance

GUADAGNO, Liberata;RAIMONDO, MARIALUIGIA;LONGO, Pasquale;
2015-01-01

Abstract

The epoxy resin has a limiting oxygen index (LOI) measured according to standard ASTM 2863, which is at least 28%, if the resin comprises at least a silsesquioxane compound (POSS), or at least 36%, if the resin is obtainable by curing an epoxy precursor formulation with an hardening agent which is an aromatic organo-phosphorous compound, preferably an organophosphine oxide of general formula R 3 PO, wherein at least two R moieties are amino-phenyl and one R moiety is alkyl, phenyl or amino-phenyl, wherein each phenyl ring may have independently one or more electrophile substituents.
2015
File in questo prodotto:
Non ci sono file associati a questo prodotto.

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/11386/4647868
 Attenzione

Attenzione! I dati visualizzati non sono stati sottoposti a validazione da parte dell'ateneo

Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus ND
  • ???jsp.display-item.citation.isi??? ND
social impact